A blast furnace burden contains 160 kg Fe,03, 54 kg SiO2, 20 kg Al,03, 100 kg CaCO3, and 78 kg C. For the smelting of the above burden, 266 Nm of air (79% N2 & 21% O2) is used. The pig iron produced...


Kindly answer the question attached:


A blast furnace burden contains 160 kg Fe,03, 54 kg SiO2, 20 kg Al,03, 100 kg CaCO3, and 78 kg C. For the<br>smelting of the above burden, 266 Nm of air (79% N2 & 21% O2) is used. The pig iron produced contains<br>4% C, 1% Si, and 95% Fe, and it is assumed that all the iron oxide is reduced to Fe. The remaining oxides<br>form a slag. Carbon in the gas is present partly as CO2 and partly as CO. Prepare as mass balance table,<br>complete with analysis of products.<br>78 kg C<br>160 kg Fe,O,<br>54 kg SiO,<br>20 kg Al,O,<br>100 kg CaCO,<br>266 Nm' dry air<br>Slag<br>(SiO, CuO, Al,0,)<br>Pig iron<br>(4% C, I % Si, 95% Fe)<br>Gas<br>(CO. CO.)<br>

Extracted text: A blast furnace burden contains 160 kg Fe,03, 54 kg SiO2, 20 kg Al,03, 100 kg CaCO3, and 78 kg C. For the smelting of the above burden, 266 Nm of air (79% N2 & 21% O2) is used. The pig iron produced contains 4% C, 1% Si, and 95% Fe, and it is assumed that all the iron oxide is reduced to Fe. The remaining oxides form a slag. Carbon in the gas is present partly as CO2 and partly as CO. Prepare as mass balance table, complete with analysis of products. 78 kg C 160 kg Fe,O, 54 kg SiO, 20 kg Al,O, 100 kg CaCO, 266 Nm' dry air Slag (SiO, CuO, Al,0,) Pig iron (4% C, I % Si, 95% Fe) Gas (CO. CO.)

Jun 11, 2022
SOLUTION.PDF

Get Answer To This Question

Related Questions & Answers

More Questions »

Submit New Assignment

Copy and Paste Your Assignment Here